The cold-rolled coil product size is accurate, uniform thickness, the thickness difference of the coil is generally not more than 0.01-0.03mm or smaller, can fully meet the requirements of high-precision tolerances.
|
3mm-2000mm or as required
|
|
|
0.1mm-300mm or as required
|
|
|
2B or according to customer requirement
|
|
|
±0.01mm
|
|
|
201, 202, 301, 302, 303, 304, 304L, 304H, 310S, 316, 316L, 317L, 321,310S 309S, 410, 410S,420, 430, 431, 440A,904L
|
|
|
|
<=1000USD, 100% in advance. Payment>=1000USD, 30% T/T in advance ,balance based on BL copy or LC at sight.If you have another question, please contact us as below
A:Different products have different delivery time.The products will be delivered as soon as possible on the basis of the quality assurance.Usually the delivery time is within5 days after we received your deposit.

It-tags Popolari: ss 304 cold rolled stainless steel coil, China ss 304 cold rolled stainless steel coil manufacturers, suppliers, factory