Id-dar-Prodotti- Azzar galvanizzat - Kojl tal-Azzar Galvanizzat-

Il-kontenut

video

DX51D Coil Z180 Zinc Coating Galvanized Steel Coil

Galvanized steel is to prevent the steel plate surface from corrosion to extend its service life, in the steel plate surface coated with a layer of metal zinc, the zinc coated steel plate are called galvanized sheet.

Introduzzjoni tal-Prodott

Introduzzjoni tal-Prodott

 

600-1500mm or as customer's requirements
0.3~6mm,or as customer's requirements
Light Oil, Unoil,dry, chromate passivated, non-chromate passivated.
DX51D, S280GD, S350GD, SGCC etc

 

3-5 Tons or as customer requirements
ISO 9001 and SGS

 

1. Q: Are you a manufacturer?


2. Q: Can we visit your factory?

3. Q: Do you have quality control system?

4. Q: Can you arrange the shipment for us?
5. Q: How long is your delivery time?
A: Generally it is 7days if we have the exact goods in our stock. If not, it will take around 15-20 days to get goods ready for delivery.
6. Q: Can I get some samples?

7. Q: What is your after-sale service?
A: We provide after-sale service and offer 100% guarantee on our products.
8. Q: What is your MOQ?
A: 1 Ton
DX51D Coil Z180 Zinc Coating Galvanized Steel Coil

It-tags Popolari: dx51d coil z180 zinc coating galvanized steel coil, China dx51d coil z180 zinc coating galvanized steel coil manufacturers, suppliers, factory

Ibgħat l-inkjesta

Ibgħat l-inkjesta