Finitura tal-kisi tal-azzar SGCD2:
R (Stangle normali), Z (Spangle minimizzat)
Kwalità tal-wiċċ tal-kolja/strixxa/folja tal-azzar SGCD2:
A (Bħala wiċċ miksi), B (wiċċ imtejjeb), C (wiċċ tal-aħjar kwalità)
Trattament tal-wiċċ tal-kolja/strixxa/folja tal-azzar SGCD2:
C (Trattament tal-kromat), NC (Trattament mhux tal-kromat), O (tħaffir taż-żejt), X (tneħħija taż-żejt) NP (Trattament ta' fosfatazzjoni ta' mhux kromat), P (Fosfat), M (Mhux trattat)
Azzar SGCD2 Massa tal-kisi tal-kolja/strixxa/folja:
Kisi taż-żingu pur: Z06 (60g), Z08(80g), Z10(100g), Z12(120g),Z14(140g),Z18(180g), Z20(200g), Z22(220g), Z25(250g), Z27 (270g), Z35(350g), Z37(370g), Z45(450g), Z60(450g)
Liga taż-żingu + Fe: F04(40g), F06(60g), F08(80g), F10(10g0), F12(120g), F18(180g)
Azzar SGCD2 Kisi tal-kolja/strixxa/folja: Z (Żingu Pur), ZF (liga Z + Fe)
JIS G 3302 azzar SGCD2 daqs adattat: Ħxuna 0.40mm-2.3mm
Kompożizzjoni kimika tal-azzar SGCD2 %:
| Grad | C massimu | Mn massimu | P massimu | S massimu |
| SGCD2 | 0.10 | 0.45 | 0.03 | 0.03 |
Azzar tal-azzar SGCD2 Proprjetajiet mekkaniċi
| Grad | Qawwa tar-Rendiment MPa | Saħħa tat-tensjoni MPa | Titwil % min | |||||
| {{0}}.25- Inqas minn jew ugwali għal 0.40mm | {{0}}.40- Inqas minn jew ugwali għal 0.60mm | {{0}}.60- Inqas minn jew ugwali għal 1.0mm | 1.0- Inqas minn jew ugwali għal 1.6mm | 1.6- Inqas minn jew ugwali għal 2.5mm | Fuq 2.5mm | |||
| SGCD2 | - | 270 min | - | 36 | 38 | 39 | 40 | - |
GNEE STEEL għandhom aktar minn 2000 tunnellata sors tal-istokk tal-azzar SGCD2 kull xahar. Nistgħu nilħqu l-biċċa l-kbira tal-kwantità u t-talba teknika tal-klijent tagħna. Ibbażat fuq dawn is-sors tal-istokk, l-industrija tal-vantaġġ tagħna tinfirex fi proċess tal-azzar bħal: qtugħ (fuq il-wisa 'u t-tul), tpinġija, ippakkjar mill-ġdid, eċċ.