Stainless steel Tees grad ekwivalenti
Stainless azzar Tees vidjo
KUMPANIJA GNEE AZZAR
Il-kumpanija tagħna hija involuta fil-produzzjoni u l-kummerċ ta 'diversi tipi ta' tees tal-istainless steel, pajpijiet tal-azzar b'forma speċjali ta 'prestazzjoni għolja u ta' preċiżjoni għolja, u pajpijiet tal-istainless steel mingħajr saldatura. Stabbilijna relazzjonijiet ta 'negozju ma' klijenti f'aktar minn 20 pajjiż u reġjun. Dettalji bħall-metodu tal-ħlas, il-ħin tal-kunsinna u l-kwantità minima jistgħu jiġu nnegozjati bbażati fuq l-ordni. Azzar tal-karbonju: ASTM A105, A350 LF2, LF3, A694 F52, F60, F65, F70
| Dijametru ta' Barra (OD) | Tee tal-pajp mingħajr saldatura (1/2″-24″), ERW/Wweldjat/Fabbricat tal-pajp Tee (1/2″-48″) |
| Dimensjonijiet | ASME/ANSI B16.9, MSS-SP-43 Tip A, MSS-SP-43 Tip B, JIS B2312, JIS B2313, ASME B16.28 |
| Ħxuna tal-ħajt | SCH5, SCH10, SCH20, SCH30, SCH40, STD, SCH80, XS, SCH60, SCH80, SCH120, SCH140, SCH160, XXS / 3mm – 40mm |
| Raġġ tal-liwi | R=1D – 10D, 15D, 20D |
| Angolu tal-Prodott | Tee ugwali, Tee mhux ugwali (Tee li Tnaqqas) |
| Servizzi ta' Valur Miżjud | Hot Dipped Galvanizzar, Epoxy & Kisi FBE, Pollakk elettro, Blasting tar-ramel, Threading, Saldjar |
| Gradi Importanti | ASTM A403 WP 304 / 304L / 304H / 316 / 316L / 317 / 317L / 321 / 310 / 347 / 904L |
| Materjali tal-Produzzjoni | Stainless Steel, Liga, Azzar tal-Karbonju, Duplex, Ligi tan-nikil, Cupro Nikil, Azzar b'Temperatura Baxxa |
| SS Punti tat-Tidwib | 1400-1450 grad (WP304, WP304L), 1390-1440 grad (WP316L), 1370 – 1400 grad (WP316) |
Stainless steel Tees jintroduċu
Tista' tikseb fehim aħjar tal-Tees ta 'l-istainless steel hawn.
Stainless steel tee huwa twaħħil tal-pajp użat fil-fergħat tal-pajpijiet. Għall-użu ta 'pajpijiet mingħajr saldatura għall-manifattura tat-tees, hemm żewġ proċessi użati b'mod komuni: projjezzjoni idrawlika u formazzjoni ta' pressa sħuna. Il-projezzjoni idrawlika tat-tees tal-istainless steel hija proċess ta 'formazzjoni li jespandi l-pajpijiet tal-fergħat permezz ta' kumpens axjali ta 'materjali tal-metall. Il-proċess huwa li tuża pressa idrawlika speċjali biex tinjetta likwidu fit-tubu vojt bl-istess dijametru bħat-tee, u agħfas it-tubu vojt permezz tal-moviment ta 'ċentru sinkroniku taż-żewġ ċilindri orizzontali tal-ġenb tal-istampa idrawlika. Il-volum tal-vojt tat-tubu jsir iżgħar wara li jiġi mbuttat, u l-parti ta 'ġewwa tal-vojt tat-tubu ssir iżgħar. Il-pressjoni tal-likwidu tiżdied hekk kif il-volum tat-tubu jsir iżgħar. Meta tintlaħaq il-pressjoni meħtieġa għall-espansjoni tal-fergħa tat-tee tal-istainless steel, il-materjal tal-metall jgħaddi tul il-kavità ta 'ġewwa tal-moffa taħt l-azzjoni doppja tal-pressjoni likwida fiċ-ċilindru tal-ġenb u t-tubu u jespandi l-fergħa. .
Il-proċess idrawliku minfuħ tat-tee ta 'l-istainless steel jista' jiġi ffurmat fi pass wieħed, u l-effiċjenza tal-produzzjoni hija għolja; tiżdied il-ħxuna tal-ħajt tal-pajp prinċipali u l-ispalla tat-tee tal-istainless steel.
Tees ta 'l-istainless steel


Stainless steel Tees element kimiku
| Buttweld Tee u Kap Daqs nominali |
Pipe Tee u Kap Barra Dijametru Y |
Pipe Tee u Kap Wall Ħxuna T |
Butweld Tee Dimensjonijiet (Ċ u M) |
Butweld Tee Piż |
Butweld Kap Tarf sa Tmiem |
Butweld Kap Piż |
||
| Mm | fi | Mm | Mm | Skeda | Mm | Mm | Mm | Kg |
| 15 | 1/2'' | 21.3 | 2.78 | STD | 25.4 | 0.58 | ||
| 3.73 | X.S | 25.4 | 0.21 | |||||
| 20 | 3/4'' | 26.7 | 2.87 | STD | 28.6 | 0.21 | ||
| 3.91 | X.S | 28.6 | 0.27 | |||||
| 25 | 1'' | 33.4 | 3.38 | STD | 38.1 | 0.34 | 38.1 | 0.1 |
| 4.55 | X.S | 38.1 | 0.43 | 38.1 | 0.14 | |||
| 32 | 11/4'' | 42.2 | 3.56 | STD | 47.6 | 0.64 | 38.1 | 0.14 |
| 4.85 | X.S | 47.6 | 0.75 | 38.1 | 0.18 | |||
| 40 | 11/2'' | 48.3 | 3.68 | STD | 57.1 | 0.95 | 38.1 | 0.18 |
| 5.08 | X.S | 57.1 | 1.13 | 38.1 | 0.23 | |||
| 50 | 2'' | 60.3 | 3.91 | STD | 63.5 | 1.45 | 38.1 | 0.27 |
| 5.54 | X.S | 63.5 | 1.72 | 38.1 | 0.32 | |||
| 65 | 21/2'' | 73.0 | 5.16 | STD | 76.2 | 2.45 | 38.1 | 0.41 |
| 7.01 | X.S | 76.2 | 2.95 | 38.1 | 0.45 | |||
| 80 | 3'' | 88.9 | 5.49 | STD | 85.7 | 3.45 | 50.8 | 0.64 |
| 7.62 | X.S | 85.7 | 4.3 | 50.8 | 0.82 | |||
| 100 | 4'' | 114.3 | 6.02 | STD | 105.0 | 5.7 | 63.5 | 1.13 |
| 8.56 | X.S | 105.0 | 7.3 | 63.5 | 1.54 | |||
| 125 | 5'' | 141.3 | 6.65 | STD | 124.0 | 9.1 | 76.2 | 1.91 |
| 9.5 | X.S | 124.0 | 11.8 | 76.2 | 2.59 | |||
| 150 | 6'' | 168.3 | 7.11 | STD | 143.0 | 13.6 | 88.9 | 2.95 |
| 10.97 | X.S | 143.0 | 19.0 | 88.9 | 4.1 | |||
| 200 | 8'' | 219.1 | 8.18 | STD | 178.0 | 25.0 | 101.6 | 5.0 |
| 12.7 | X.S | 178.0 | 33.5 | 101.6 | 7.3 | |||
| 250 | 10'' | 273.0 | 9.27 | STD | 216.0 | 41.0 | 127.0 | 9.1 |
| 12.7 | X.S | 216.0 | 54.0 | 127.0 | 12.0 | |||
| 300 | 12'' | 323.9 | 9.52 | STD | 254.0 | 57.0 | 152.4 | 13.6 |
| 12.7 | X.S | 254.0 | 77.0 | 152.4 | 17.0 | |||
| 350 | 14'' | 355.6 | 9.52 | STD | 279.0 | 73.0 | 165.1 | 15.9 |
| 12.7 | X.S | 279.0 | 93.0 | 165.1 | 21.0 | |||
| 400 | 16'' | 406.4 | 9.52 | STD | 305.0 | 91.0 | 178.8 | 20.0 |
| 12.7 | X.S | 305.0 | 120.0 | 178.8 | 26.0 | |||
| 450 | 18'' | 457.0 | 9.52 | STD | 343.0 | 127.0 | 203.2 | 26.0 |
| 12.7 | X.S | 343.0 | 165.0 | 203.2 | 34.0 | |||
| 500 | 20'' | 508.0 | 9.52 | STD | 381.0 | 227.0 | 228.6 | 33.0 |
| 12.7 | X.S | 381.0 | 270.0 | 228.6 | 43.0 | |||
| 600 | 24'' | 610.0 | 9.52 | STD | 432.0 | 345.0 | 266.7 | 46.0 |
| 12.7 | X.S | 432.0 | 430.0 | 266.7 | 61.0 | |||
Tees ta 'l-istainless steel


Fuqna
Tista' titgħallem aktar dwar Gnee hawn.
Il-klijenti barranin iżuru

FAQ
Q: Nista 'nikseb l-aħjar prezz tiegħek?
A: L-għan tagħna huwa li nipprovdulek l-aħjar prezz u assigurazzjoni ta 'kwalità eċċellenti fit-tul. Jekk jogħġbok ħalli l-informazzjoni ta 'kuntatt tiegħek biex tikseb l-aħjar kwotazzjoni, aħna nipprovdulek l-aħjar soluzzjoni kemm jista' jkun malajr.
Q: Kemm huwa twil il-ħin tal-kunsinna tiegħek?
A: Ġeneralment huwa 5-10 ijiem jekk il-merkanzija tkun fl-istokk. Jew jekk l-oġġetti mhumiex fl-istokk, huma 15-20 jiem, skont il-kwantità.
Q: tipprovdi kampjuni? Huwa b'xejn jew żejjed?
A: Iva, nistgħu nipprovdu kampjuni b'xejn mingħajr ma nħallsu l-ispiża tat-tbaħħir.
Q: About Stainless steel Tees prezzijiet tal-prodott?
A: Il-prezzijiet ivarjaw minn perjodu għal perjodu minħabba bidliet ċikliċi fil-prezz tal-materja prima.
Ikkuntatjana
Maniġer tat-Tees tal-istainless steel

It-tags Popolari: tees tal-istainless steel, manifatturi taċ-Ċina tees tal-istainless steel, fornituri, fabbrika